Gasket cement

da.bees

Well-known Member
To use or not to use cement with paper gaskets. In this case tractor engine water pump. Lots of people butter gaskets with RTV on everything besides hydraulics saying they don't want to risk squeeze out getting into hydraulic system. I figure if dry paper can hold extreme hydraulic pressure it should hold anywhere. I'm leaning toward grease or dry unless surface is rough or pitted then I say butter with RTV. What's your opinion?

This post was edited by da.bees on 08/07/2021 at 07:48 pm.
 
Rtv works fine for most stuff, the newer stuff is much tougher than the stuff we had 20 years ago. But use it sparingly just a thin film, as you say pushing out can be a real issue. I saw an engine plug an oil hole with rtv residue and ruin a rod bearing
 
(quoted from post at 23:20:31 08/07/21) Spray copper coat
I'll try that when i have a complete engine to assemble. I'm fresh out of spray copper and it seem's such a waste to make a trip for one little paper gasket. :( [/img:8ac30bd456]
 

Water pump gaskets.

I stick the paper to the pump with 3M Yellow Super Weatherstrip and Gasket Adhesive, 08002. Then smear a very light coating of Permatex ultra grey on the engine side of the gasket. Have all your ducks in a row be ready to install the gasket.

When you put the adhesive on the pump apply the gasket then remove it for 30 sec are so then put the gasket back on. It will then be stuck and wont move on ya.

Why do I do this if I ever have to remove the pump its easier to remove any gasket are RTV from the surface than stuck paper that's hard as a brick. Its also a little insurance : )

Folks say that weatherstrip is a pain to remove I say its a lot easier when you have the part in your hand versed in a hole that's hard to get to.

That's the way I have done it for a many decade so far so good. When I get a hold of one where they used the other recommendations I am PIZZZZED...
 
If surfaces are good and flat I use a gasket if I have one. If I dont have the gasket, then its anaerobic gasket maker. This stuff only hardens when it is clamped together so any that pushes out is a non issue.

I only use RTV occasionally, and then its a minimal amount. Never in the butter amount.
 
I like Permatex too. I never had a wetted gasked fail, nor have to go back and retorque, being it a head gasket (Copper Coat aerosol), water pump or whatever (Permatex 1,2, or 3 depending on the application). Had numerous dry fail and that's why I started wetting them. Biggest problem was automatic transmission pan sealing. Finally resolved that problem with Permatex 3 but only painting one side of the cork gasket, not both.
 
RTV. But, I do it different than most. I keep a box of the thinnest, cheapest vinyl gloves I can find in my toolbox. Using those on my hands I coat both sides of paper gaskets with a really thin coat and install. No squeeze-out to worry about due to the light coat.

Head gaskets get either spray copper-coat or aluminum paint, depending on the gasket style.

Cork gaskets get the RTV treatment + a little dab at corners where gaskets meet.

Bolts into water passages get threads treated with Permatex #2.
 
My suggestion is to use a thin film of gasket compound on the side of the gasket that goes against the part that can be removed and put on a workbench (in this case, the water pump), and a thin film of grease, oil, or non-hardening pipe joint compound containing PTFE on the side of the gasket that fits against the part that stays in the machine. This makes it MUCH easier to do the next disassembly and cleaning MUCH easier.
 
Ol Yeller,I didn't think anyone still used that stuff for gaskets. I recall when every mechanic had a tube,sometimes 2 or 3 in their tool box. They used it often and generously until they began having to disassemble and get it off later on. It was so despised shops wouldn't quote flat rate and if they did,a disclaimer was noted on work order in the event it was found during tear down. I had no idea Permatex had so many specialized products until I went to their site to look at specs for #2. I don't have a head gasket job at the moment but have a question about copper coating. Is it used for better seal or for heat transfer?
 

knuckleheads' will screw up anything... If a little is OK then a lot has got to be better...

"It was so despised" I never heard anyone say that we must live in different worlds... Part of the gig is repairing it we may not like what the other guy did but its part of the gig...

Of course we can always say NO! and fire the customer : 0
 
Some Harley gaskets are made to be greased. Usually black in appearance . Hylomar is over -rated.Aviation Permatex or High Tack is all I use If it's good enough for aircraft... Silicone is for something else besides gasket sealer just clogs stuff up.
 