Welding question

I bought a rough scrape blade a year or so ago for $75 and, although lots of rust, it seems to work OK. However, the vertical tube on the back has split at the corner of the tube (will try to post a pic). I'm not competent to weld the split so was thinking I'd weld a piece of 1/4" thick x 2 x 2" angle on the corner to secure it. Basically wrap the corner with the piece of angle. My welder is a 120v stick welder with which I've done some minor welding repairs and built a welder cart. I have E6011 and E7014 welding rods on hand. Question is, would a 120v stick welder work with this repair given the rust of the tube and the stress the tube is likely to incur? And, which welding rod would be the best to do the job? Thanks.
mvphoto52842.jpg
 
Most important tool you need is a grinder. Grind the rust back both sides and down into the crack as best you can. Use your 6011, will work fine. You
will need multiple passes with your little welder, and assume you have an appropriate size rod like 3/32. If you have a torch to add some heat to the
steel before you weld it will help also.

All that said, I bet you could ignore the crack and it will make no difference for your uses.
 
I would like to see the other side of that, I don't think it is a
tube. Looks more like a poor patch job from that side. Not that
it matters much. You can weld that with your welder but it will
be at the max to do it. As said, grind it down so the rust is
gone first. Then I would hammer the side in to close the gap
and weld the gap shut. But that advice might change if I saw a
pic or two from different angles. 6011 is fine for that, so would 6013 and it is a bit easier to weld with for beginners. 7014 is ok too as long as it's ground clean.
 
I don't see why you can't fill that crack,and then weld the angle iron over it to beef it up.i would be sure to prep that real good,and your welder should handle it on the highest setting.you can use either rod but the 7014s will be stronger.
 
Thanks for everyone's advice. The other corner of the tube is not split but my plan was to run a piece of angle on that corner also since I figure a split is just a matter of time. I figured that I'd have to grind back to bare steel and also hit one side of the split to push that side back to improve alignment. I'm glad to hear that you think my 120v welder is up to the task.

I'm curious to know what are the benefits of the E6011 vs. E7014 welding rods? Is the amount of rust and rot a determining factor in picking the best rod or are there other reasons?

Thanks
 
I'm NOT a pro welder but I've laid many a bead that are still holding. I was taught that E6011 rods were for deep penetration in rusty metal and E7014 rods were for 'purdy' welds on clean metal. That being said, lay a bead of E6011, clean it, then weld a E7014 over top of it and see how it looks. However you decide to do it should be fine for your use. Good Luck with it!
 
Jobs like that is where the 6011 shines.
Don't forget to clean off the slag
between passes & you'll be fine. I don't
think it's a split tube either. Looks
more like a channel and plate to me.
Nothing wrong with that either if it's
welded decent.

I'm partial to the 6011 because that's
what I started with after talking with
the guys at the scrap yard. Turn the heat
up and it will hold. Might not be pretty
until you get a lot of practice in but it
will hold. Farm repair ain't about
pretty, it's about holding!
 
Your competence with any rod is more important than the quality of the rod. 6011 is right for the job on mild steel and you shall do well. I do not think you need an angle for reinforcement. Two passes with 6011 shall give you more strength than the original metal.
 
7014 is for flat clean welds. It's a drag rod so you tap the rid
on the metal and drag it along as apposed to raising it to create
the arc. That makes it very easy to use and get a good bead.
It would be a good rid for this. 6011 is the old standby and an
excellent rod. It does handle dirty metal better and penetrate
better. With your welder being taxed for this the extra
penetration might be helpful. However, a good weld with any
rod is better than a poor weld with any rod. 6011 is harder to
use than either 7014 or 6013 so therefore be careful. Most
will say 6013 is not as good but it's easier to use than 6011
and can be used in all positions. The truth is that very few
people on this site have either the skills or equipment to make
use of the differences in rods, so choose the one that works
best for you and go to work.
 
To go along with what others have said, I find it helpful to mock up a similar weld with scrap material and practice a little before I weld the actual project.
 
Your 120 volt welder will need all the help it can get. 6011 is your friend here; not only will it handle rusty steel, it will give deeper penetration with your welder's limited output than pretty much anything else. And once you do the root pass with 6011, you can always use your 7014 for a second pass to make it all purty.

Practice with the 6011 if you haven't used it before; it's not an easy electrode to use. It's often used with "whip and pause" technique; you can google to find plenty of videos about whip and pause. And clean up as much rust on your work as you can before you start.

I'm guessing your electrodes have been lying around for awhile. If they haven't been in sealed containers you should be aware of the effects of moisture content. 6011 (and its cousin 6010) luvs moisture. If you're in a dry climate your 6011 may need to soak in water a bit to work well. Most other electrodes don't do well when wet; if you're in a damp climate you should probably bake your 7014 before you try to use it.
 
You have some good advise but I will add that it might help if you made a few test beads on similar thickness scrap before you try for the important one if you aren't
familiar with how the welder and the welder will work out. If it looks like you don't have enough heat, (base metal not melting and welds look like little balls of metal
not a smooth bead) then you might try pre heating the job if you have a way, even building a fire under it long as you clean off the smoke before welding. Especially if
it is cold getting it up to even 100 or 150 degrees can help.
 
I agree with the other posts that advises you to grind it to
clean up the rust and then use 6011. With the 110v welder
you may have better luck with the smaller rod (3/32?).
 
Be aware that some 120V welders have a short duty cycle. That means is can't put out full power continuously nonstop without it overheating. So you may need to weld a bead for 30 seconds, then stop and clean the metal for a minute or 2, just to let the welder rest and cool down a little.
 
Man, I'd be really happy if I was able to run a bead for as long as 30 seconds. I appreciate everyone's confidence in my welding skills and hope not to disappoint. Am gonna get out the grinder and the stick welder this weekend and give it a try. Good or bad, I'll post back with results. Thanks.
 